The effect of the calcination temperature and composition of the MnOx–ZrO2 system on its structural characteristics and catalytic properties in the reaction of CO oxidation was studied. According to X-ray diffraction analysis and H2 thermo-programmed reduction data, an increase in the calcination temperature of Mn0.12Zr0.88O2 from 450 to 900°C caused a structural transformation of the system accompanied by the disintegration of solid solution with the release of manganese ions from the structure of ZrO2 and the formation of, initially, highly dispersed MnOx particles and then a crystallized phase of Mn3O4. The dependence of the catalytic activity of MnOx–ZrO2 in the reaction of CO oxidation on the calcination temperature takes an extreme form. A maximum activity was observed after heat treatment at 650–700°C, i.e., at limiting temperatures for the occurrence of a solid solution of manganese ions in the cubic modification of ZrO2. If the manganese content was higher than that in the sample of Mn0.4Zr0.6O2, the phase composition of the system changed: the solid solution phase was supplemented with Mn2O3 and β-Mn3O4 phases. The samples of Mn0.4Zr0.6O2–Mn0.6Zr0.4O2 exhibited a maximum catalytic activity; this was likely due to the presence of the highly dispersed MnOx particles, which were not the solid solution constituents, on their surface in addition to an increase in the dispersity of the solid solution. More... »

PAGES

104-111

Identifiers

URI

http://scigraph.springernature.com/pub.10.1134/s0023158418010019

DOI

http://dx.doi.org/10.1134/s0023158418010019

DIMENSIONS

https://app.dimensions.ai/details/publication/pub.1101344460


Indexing Status Check whether this publication has been indexed by Scopus and Web Of Science using the SN Indexing Status Tool
Incoming Citations Browse incoming citations for this publication using opencitations.net

JSON-LD is the canonical representation for SciGraph data.

TIP: You can open this SciGraph record using an external JSON-LD service: JSON-LD Playground Google SDTT

[
  {
    "@context": "https://springernature.github.io/scigraph/jsonld/sgcontext.json", 
    "about": [
      {
        "id": "http://purl.org/au-research/vocabulary/anzsrc-for/2008/03", 
        "inDefinedTermSet": "http://purl.org/au-research/vocabulary/anzsrc-for/2008/", 
        "name": "Chemical Sciences", 
        "type": "DefinedTerm"
      }, 
      {
        "id": "http://purl.org/au-research/vocabulary/anzsrc-for/2008/0306", 
        "inDefinedTermSet": "http://purl.org/au-research/vocabulary/anzsrc-for/2008/", 
        "name": "Physical Chemistry (incl. Structural)", 
        "type": "DefinedTerm"
      }
    ], 
    "author": [
      {
        "affiliation": {
          "alternateName": "Institute of Hydrocarbon Processing, Siberian Branch, Russian Academy of Sciences, 644040, Omsk, Russia", 
          "id": "http://www.grid.ac/institutes/grid.465467.2", 
          "name": [
            "Institute of Hydrocarbon Processing, Siberian Branch, Russian Academy of Sciences, 644040, Omsk, Russia"
          ], 
          "type": "Organization"
        }, 
        "familyName": "Afonasenko", 
        "givenName": "T. N.", 
        "id": "sg:person.014665447153.39", 
        "sameAs": [
          "https://app.dimensions.ai/discover/publication?and_facet_researcher=ur.014665447153.39"
        ], 
        "type": "Person"
      }, 
      {
        "affiliation": {
          "alternateName": "Novosibirsk State University, 630090, Novosibirsk, Russia", 
          "id": "http://www.grid.ac/institutes/grid.4605.7", 
          "name": [
            "Boreskov Institute of Catalysis, Siberian Branch, Russian Academy of Sciences, 630090, Novosibirsk, Russia", 
            "Novosibirsk State University, 630090, Novosibirsk, Russia"
          ], 
          "type": "Organization"
        }, 
        "familyName": "Bulavchenko", 
        "givenName": "O. A.", 
        "id": "sg:person.013513771252.46", 
        "sameAs": [
          "https://app.dimensions.ai/discover/publication?and_facet_researcher=ur.013513771252.46"
        ], 
        "type": "Person"
      }, 
      {
        "affiliation": {
          "alternateName": "Institute of Hydrocarbon Processing, Siberian Branch, Russian Academy of Sciences, 644040, Omsk, Russia", 
          "id": "http://www.grid.ac/institutes/grid.465467.2", 
          "name": [
            "Institute of Hydrocarbon Processing, Siberian Branch, Russian Academy of Sciences, 644040, Omsk, Russia"
          ], 
          "type": "Organization"
        }, 
        "familyName": "Gulyaeva", 
        "givenName": "T. I.", 
        "id": "sg:person.012276266654.69", 
        "sameAs": [
          "https://app.dimensions.ai/discover/publication?and_facet_researcher=ur.012276266654.69"
        ], 
        "type": "Person"
      }, 
      {
        "affiliation": {
          "alternateName": "Novosibirsk State University, 630090, Novosibirsk, Russia", 
          "id": "http://www.grid.ac/institutes/grid.4605.7", 
          "name": [
            "Boreskov Institute of Catalysis, Siberian Branch, Russian Academy of Sciences, 630090, Novosibirsk, Russia", 
            "Novosibirsk State University, 630090, Novosibirsk, Russia"
          ], 
          "type": "Organization"
        }, 
        "familyName": "Tsybulya", 
        "givenName": "S. V.", 
        "id": "sg:person.011252704043.40", 
        "sameAs": [
          "https://app.dimensions.ai/discover/publication?and_facet_researcher=ur.011252704043.40"
        ], 
        "type": "Person"
      }, 
      {
        "affiliation": {
          "alternateName": "Institute of Hydrocarbon Processing, Siberian Branch, Russian Academy of Sciences, 644040, Omsk, Russia", 
          "id": "http://www.grid.ac/institutes/grid.465467.2", 
          "name": [
            "Institute of Hydrocarbon Processing, Siberian Branch, Russian Academy of Sciences, 644040, Omsk, Russia"
          ], 
          "type": "Organization"
        }, 
        "familyName": "Tsyrul\u2019nikov", 
        "givenName": "P. G.", 
        "id": "sg:person.010322770105.18", 
        "sameAs": [
          "https://app.dimensions.ai/discover/publication?and_facet_researcher=ur.010322770105.18"
        ], 
        "type": "Person"
      }
    ], 
    "datePublished": "2018-01", 
    "datePublishedReg": "2018-01-01", 
    "description": "The effect of the calcination temperature and composition of the MnOx\u2013ZrO2 system on its structural characteristics and catalytic properties in the reaction of CO oxidation was studied. According to X-ray diffraction analysis and H2 thermo-programmed reduction data, an increase in the calcination temperature of Mn0.12Zr0.88O2 from 450 to 900\u00b0C caused a structural transformation of the system accompanied by the disintegration of solid solution with the release of manganese ions from the structure of ZrO2 and the formation of, initially, highly dispersed MnOx particles and then a crystallized phase of Mn3O4. The dependence of the catalytic activity of MnOx\u2013ZrO2 in the reaction of CO oxidation on the calcination temperature takes an extreme form. A maximum activity was observed after heat treatment at 650\u2013700\u00b0C, i.e., at limiting temperatures for the occurrence of a solid solution of manganese ions in the cubic modification of ZrO2. If the manganese content was higher than that in the sample of Mn0.4Zr0.6O2, the phase composition of the system changed: the solid solution phase was supplemented with Mn2O3 and \u03b2-Mn3O4 phases. The samples of Mn0.4Zr0.6O2\u2013Mn0.6Zr0.4O2 exhibited a maximum catalytic activity; this was likely due to the presence of the highly dispersed MnOx particles, which were not the solid solution constituents, on their surface in addition to an increase in the dispersity of the solid solution.", 
    "genre": "article", 
    "id": "sg:pub.10.1134/s0023158418010019", 
    "inLanguage": "en", 
    "isAccessibleForFree": false, 
    "isPartOf": [
      {
        "id": "sg:journal.1136331", 
        "issn": [
          "0023-1584", 
          "0453-8811"
        ], 
        "name": "Kinetics and Catalysis", 
        "publisher": "Pleiades Publishing", 
        "type": "Periodical"
      }, 
      {
        "issueNumber": "1", 
        "type": "PublicationIssue"
      }, 
      {
        "type": "PublicationVolume", 
        "volumeNumber": "59"
      }
    ], 
    "keywords": [
      "calcination temperature", 
      "CO oxidation", 
      "catalytic properties", 
      "catalytic activity", 
      "manganese ions", 
      "carbon monoxide oxidation", 
      "solid solution", 
      "structure of ZrO2", 
      "maximum catalytic activity", 
      "ray diffraction analysis", 
      "Mn3O4 phase", 
      "MnOx particles", 
      "solution phase", 
      "diffraction analysis", 
      "solution constituents", 
      "oxidation", 
      "solid solution phase", 
      "phase composition", 
      "crystallized phase", 
      "structural transformation", 
      "reaction", 
      "ions", 
      "structural characteristics", 
      "ZrO2", 
      "cubic modification", 
      "solid solution constituents", 
      "MnOx", 
      "maximum activity", 
      "Mn3O4", 
      "Mn2O3", 
      "dispersity", 
      "solution", 
      "heat treatment", 
      "properties", 
      "temperature", 
      "composition", 
      "manganese content", 
      "structure", 
      "phase", 
      "reduction data", 
      "surface", 
      "particles", 
      "formation", 
      "activity", 
      "samples", 
      "constituents", 
      "modification", 
      "release", 
      "presence", 
      "dependence", 
      "system", 
      "transformation", 
      "effect", 
      "addition", 
      "disintegration", 
      "content", 
      "increase", 
      "form", 
      "analysis", 
      "characteristics", 
      "treatment", 
      "occurrence", 
      "data", 
      "extreme form"
    ], 
    "name": "Effect of the Calcination Temperature and Composition of the MnOx\u2013ZrO2 System on Its Structure and Catalytic Properties in a Reaction of Carbon Monoxide Oxidation", 
    "pagination": "104-111", 
    "productId": [
      {
        "name": "dimensions_id", 
        "type": "PropertyValue", 
        "value": [
          "pub.1101344460"
        ]
      }, 
      {
        "name": "doi", 
        "type": "PropertyValue", 
        "value": [
          "10.1134/s0023158418010019"
        ]
      }
    ], 
    "sameAs": [
      "https://doi.org/10.1134/s0023158418010019", 
      "https://app.dimensions.ai/details/publication/pub.1101344460"
    ], 
    "sdDataset": "articles", 
    "sdDatePublished": "2022-05-20T07:35", 
    "sdLicense": "https://scigraph.springernature.com/explorer/license/", 
    "sdPublisher": {
      "name": "Springer Nature - SN SciGraph project", 
      "type": "Organization"
    }, 
    "sdSource": "s3://com-springernature-scigraph/baseset/20220519/entities/gbq_results/article/article_786.jsonl", 
    "type": "ScholarlyArticle", 
    "url": "https://doi.org/10.1134/s0023158418010019"
  }
]
 

Download the RDF metadata as:  json-ld nt turtle xml License info

HOW TO GET THIS DATA PROGRAMMATICALLY:

JSON-LD is a popular format for linked data which is fully compatible with JSON.

curl -H 'Accept: application/ld+json' 'https://scigraph.springernature.com/pub.10.1134/s0023158418010019'

N-Triples is a line-based linked data format ideal for batch operations.

curl -H 'Accept: application/n-triples' 'https://scigraph.springernature.com/pub.10.1134/s0023158418010019'

Turtle is a human-readable linked data format.

curl -H 'Accept: text/turtle' 'https://scigraph.springernature.com/pub.10.1134/s0023158418010019'

RDF/XML is a standard XML format for linked data.

curl -H 'Accept: application/rdf+xml' 'https://scigraph.springernature.com/pub.10.1134/s0023158418010019'


 

This table displays all metadata directly associated to this object as RDF triples.

154 TRIPLES      21 PREDICATES      90 URIs      82 LITERALS      6 BLANK NODES

Subject Predicate Object
1 sg:pub.10.1134/s0023158418010019 schema:about anzsrc-for:03
2 anzsrc-for:0306
3 schema:author N40a32f9c890e44beab8efafc39556a79
4 schema:datePublished 2018-01
5 schema:datePublishedReg 2018-01-01
6 schema:description The effect of the calcination temperature and composition of the MnOx–ZrO2 system on its structural characteristics and catalytic properties in the reaction of CO oxidation was studied. According to X-ray diffraction analysis and H2 thermo-programmed reduction data, an increase in the calcination temperature of Mn0.12Zr0.88O2 from 450 to 900°C caused a structural transformation of the system accompanied by the disintegration of solid solution with the release of manganese ions from the structure of ZrO2 and the formation of, initially, highly dispersed MnOx particles and then a crystallized phase of Mn3O4. The dependence of the catalytic activity of MnOx–ZrO2 in the reaction of CO oxidation on the calcination temperature takes an extreme form. A maximum activity was observed after heat treatment at 650–700°C, i.e., at limiting temperatures for the occurrence of a solid solution of manganese ions in the cubic modification of ZrO2. If the manganese content was higher than that in the sample of Mn0.4Zr0.6O2, the phase composition of the system changed: the solid solution phase was supplemented with Mn2O3 and β-Mn3O4 phases. The samples of Mn0.4Zr0.6O2–Mn0.6Zr0.4O2 exhibited a maximum catalytic activity; this was likely due to the presence of the highly dispersed MnOx particles, which were not the solid solution constituents, on their surface in addition to an increase in the dispersity of the solid solution.
7 schema:genre article
8 schema:inLanguage en
9 schema:isAccessibleForFree false
10 schema:isPartOf Nb393dbb0d2424d33afe422d9920a9d68
11 Nfd3da8ed3740421fb838b4a00e0ff3d0
12 sg:journal.1136331
13 schema:keywords CO oxidation
14 Mn2O3
15 Mn3O4
16 Mn3O4 phase
17 MnOx
18 MnOx particles
19 ZrO2
20 activity
21 addition
22 analysis
23 calcination temperature
24 carbon monoxide oxidation
25 catalytic activity
26 catalytic properties
27 characteristics
28 composition
29 constituents
30 content
31 crystallized phase
32 cubic modification
33 data
34 dependence
35 diffraction analysis
36 disintegration
37 dispersity
38 effect
39 extreme form
40 form
41 formation
42 heat treatment
43 increase
44 ions
45 manganese content
46 manganese ions
47 maximum activity
48 maximum catalytic activity
49 modification
50 occurrence
51 oxidation
52 particles
53 phase
54 phase composition
55 presence
56 properties
57 ray diffraction analysis
58 reaction
59 reduction data
60 release
61 samples
62 solid solution
63 solid solution constituents
64 solid solution phase
65 solution
66 solution constituents
67 solution phase
68 structural characteristics
69 structural transformation
70 structure
71 structure of ZrO2
72 surface
73 system
74 temperature
75 transformation
76 treatment
77 schema:name Effect of the Calcination Temperature and Composition of the MnOx–ZrO2 System on Its Structure and Catalytic Properties in a Reaction of Carbon Monoxide Oxidation
78 schema:pagination 104-111
79 schema:productId N6238464384c2470a975ae1fbbea89c63
80 N7096d250cd0d40c79df2bc0b2ac1ebd0
81 schema:sameAs https://app.dimensions.ai/details/publication/pub.1101344460
82 https://doi.org/10.1134/s0023158418010019
83 schema:sdDatePublished 2022-05-20T07:35
84 schema:sdLicense https://scigraph.springernature.com/explorer/license/
85 schema:sdPublisher Ncce01021173a4d008e34ee6d4209d66a
86 schema:url https://doi.org/10.1134/s0023158418010019
87 sgo:license sg:explorer/license/
88 sgo:sdDataset articles
89 rdf:type schema:ScholarlyArticle
90 N0d2daf54a5cc446d9e2a5a82b016ef06 rdf:first sg:person.010322770105.18
91 rdf:rest rdf:nil
92 N40a32f9c890e44beab8efafc39556a79 rdf:first sg:person.014665447153.39
93 rdf:rest Nb73ab63cd7b246d4a86235b0bc041ff6
94 N6238464384c2470a975ae1fbbea89c63 schema:name doi
95 schema:value 10.1134/s0023158418010019
96 rdf:type schema:PropertyValue
97 N7096d250cd0d40c79df2bc0b2ac1ebd0 schema:name dimensions_id
98 schema:value pub.1101344460
99 rdf:type schema:PropertyValue
100 Nb393dbb0d2424d33afe422d9920a9d68 schema:volumeNumber 59
101 rdf:type schema:PublicationVolume
102 Nb73ab63cd7b246d4a86235b0bc041ff6 rdf:first sg:person.013513771252.46
103 rdf:rest Nfd4389959e774a9fb193f7eaf064f483
104 Ncce01021173a4d008e34ee6d4209d66a schema:name Springer Nature - SN SciGraph project
105 rdf:type schema:Organization
106 Nf4ed88f81bf0429b9179f3b16747499a rdf:first sg:person.011252704043.40
107 rdf:rest N0d2daf54a5cc446d9e2a5a82b016ef06
108 Nfd3da8ed3740421fb838b4a00e0ff3d0 schema:issueNumber 1
109 rdf:type schema:PublicationIssue
110 Nfd4389959e774a9fb193f7eaf064f483 rdf:first sg:person.012276266654.69
111 rdf:rest Nf4ed88f81bf0429b9179f3b16747499a
112 anzsrc-for:03 schema:inDefinedTermSet anzsrc-for:
113 schema:name Chemical Sciences
114 rdf:type schema:DefinedTerm
115 anzsrc-for:0306 schema:inDefinedTermSet anzsrc-for:
116 schema:name Physical Chemistry (incl. Structural)
117 rdf:type schema:DefinedTerm
118 sg:journal.1136331 schema:issn 0023-1584
119 0453-8811
120 schema:name Kinetics and Catalysis
121 schema:publisher Pleiades Publishing
122 rdf:type schema:Periodical
123 sg:person.010322770105.18 schema:affiliation grid-institutes:grid.465467.2
124 schema:familyName Tsyrul’nikov
125 schema:givenName P. G.
126 schema:sameAs https://app.dimensions.ai/discover/publication?and_facet_researcher=ur.010322770105.18
127 rdf:type schema:Person
128 sg:person.011252704043.40 schema:affiliation grid-institutes:grid.4605.7
129 schema:familyName Tsybulya
130 schema:givenName S. V.
131 schema:sameAs https://app.dimensions.ai/discover/publication?and_facet_researcher=ur.011252704043.40
132 rdf:type schema:Person
133 sg:person.012276266654.69 schema:affiliation grid-institutes:grid.465467.2
134 schema:familyName Gulyaeva
135 schema:givenName T. I.
136 schema:sameAs https://app.dimensions.ai/discover/publication?and_facet_researcher=ur.012276266654.69
137 rdf:type schema:Person
138 sg:person.013513771252.46 schema:affiliation grid-institutes:grid.4605.7
139 schema:familyName Bulavchenko
140 schema:givenName O. A.
141 schema:sameAs https://app.dimensions.ai/discover/publication?and_facet_researcher=ur.013513771252.46
142 rdf:type schema:Person
143 sg:person.014665447153.39 schema:affiliation grid-institutes:grid.465467.2
144 schema:familyName Afonasenko
145 schema:givenName T. N.
146 schema:sameAs https://app.dimensions.ai/discover/publication?and_facet_researcher=ur.014665447153.39
147 rdf:type schema:Person
148 grid-institutes:grid.4605.7 schema:alternateName Novosibirsk State University, 630090, Novosibirsk, Russia
149 schema:name Boreskov Institute of Catalysis, Siberian Branch, Russian Academy of Sciences, 630090, Novosibirsk, Russia
150 Novosibirsk State University, 630090, Novosibirsk, Russia
151 rdf:type schema:Organization
152 grid-institutes:grid.465467.2 schema:alternateName Institute of Hydrocarbon Processing, Siberian Branch, Russian Academy of Sciences, 644040, Omsk, Russia
153 schema:name Institute of Hydrocarbon Processing, Siberian Branch, Russian Academy of Sciences, 644040, Omsk, Russia
154 rdf:type schema:Organization
 




Preview window. Press ESC to close (or click here)


...